Wave spring is a thin ring-shaped elastic metal element composed of several wave crests and valleys. Wave springs are widely used in motors, textile machinery, hydraulic equipment, automobiles and other industries. The main installation and specifications (nominal size) of the bearing room are suitable. Or in the hole, the installation space is small, and it has the special function of reducing noise and reducing vibration.
The outer diameter ranges from 6mm to 1000mm.the thickness ranges from 0.4mm to 5.0mm.
• High Tempeature Spring Materials:
SUS304,SUS316, SUS631/17-7PH, SUS632/15-7Mo, 50CrVA, 30W4Cr2VA,
Inconel X-750, Inconel 718, Nimonic90, Incoloy A286(SUH660)
• Spring Types:
→Compression Springs →Extension spring
→Torsion Spring →Bending spring
♦ Wave Spring ♦ Scroll Spring ♦ Disc Spring
♦ Ring Spring ♦ Special-Shaped Spring, etc
Material Types |
Material Name |
Maximum Application temperature°C |
stainless steel |
SUS304/SUS316 |
200 |
SUS631/17-7PH |
370 |
|
SUS632/15-7Mo |
470 |
|
Alloy spring steel |
50CrVA |
300 |
30W4Cr2VA |
500 |
|
High temperature nickel base alloy |
Incoloy A286(GH2132) |
600 |
Inconel X-750(GH4145) |
600 |
|
Inconel 718 (GH4169) |
690 |
|
Nimonic90(GH4090) |
800 (γ<0.2) |
|
GH4099 |
1000 (γ<0.1) |
They are mainly used in valves, flanges, clutches, brakes, torque converters, High-voltage switch, bolt tightening, pipeline support, shockproof and shockproof fields. they produced in accordance with DIN EN16983 (DIN2093).
The outer diameter ranges from 6mm to 1000mm.
The materials include alloy steel 51CrV4, carbon steel SK85, 1074;
• Stainless steel ASTM301, 304, 316, 17-7PH, 17-4PH, 15-7Mo;
• Heat-resistant steel H13, X30WCrV53, X22CrMoV12-1, X39CrMo17-1;
• High temperature resistant stainless steel Inconel X750, Inconel X718, Nimonic 90, etc.
They have the characteristics of small deformation and large load. It also has the following features.
Spring Materials | Work Temp | Tensile Strength | Elastic Modulus KN//mm2 | Chemistry% | ||||||||||||||||||
°C | N/mm2 | RT°C | 100°C | 200°C | 300°C | 400°C | 500°C | 600°C | C | Si | Mn | P | S | Cr | Ni | Others |
||||||
T8A SK85 |
-50 to +100 | 1200-1800 | 206 | 202 | - | - | - | - | - | 0.80-0.09 | ≤ 0.35 | ≤ 0.50 | ≤ 0.03 | ≤ 0.03 | ≤ 0.20 | ≤ 0.25 | Cu≤0.30 | |||||
50CrV4 SUP10 |
-50 to +200 | 1200-1800 | 206 | 202 | 196 | - | - | - | - | 0.47-0.55 | ≤ 0.4 | 0.7 1.1 | ≤ 0.025 | 0.025 | 0.9 1.2 | ≤ 0.4 | V:0.1 0.25 Mo≤ 0.1 | |||||
C75 | -50 to +100 | 1200-1800 | 206 | 202 | - | - | - | - | - | 0.70-0.80 | 0.15-0.35 | 0.60 0.90 | ≤ 0.025 | 0.025 | ≤ 0.4 | ≤ 0.4 | Mo≤ 0.1 | |||||
60Si2Mn SUP6 | -50 to +200 | 1200-1800 | 206 | 202 | 196 | - | - | - | - | 0.56-0.64 | 1.50-2.0 | 0.6 0.9 | ≤ 0.035 | 0.035 | ≤ 0.35 | ≤ 0.35 | ||||||
X 10CrNi 18-8 SUS301 | -200 to +200 | 1150-1500 | 190 | 186 | 180 | - | - | - | - | 0.05-0.15 | ≤ 2.0 | ≤ 2.0 | ≤ 0.045 | 0.015 | 16.0 19.0 | 6.0 9.5 | Mo≤ 0.08 | |||||
X 5CrNi 18-10SUS304 | -200 to +200 | 1000-1500 | 185 | 179 | 171 | - | - | - | - | ≤ 0.07 | ≤ 1.0 | ≤ 2.0 | ≤ 0.045 | 0.015 | 17.0 19.5 | 6.0 9.5 | N≤ 0.11 |
|||||
X 5CrNiMo 17-12-2 SUS316 | -200 to +200 | 1000-1500 | 180 | 176 | 171 | - | - | - | - | ≤ 0.07 | ≤ 1.0 | ≤ 2.0 | ≤ 0.045 | 0.015 | 16.5-18.5 | 10.0 13.0 | Mo:2.0-2.5 N≤ 0.11 | |||||
X 7CrNiAl 17-7 SUS631 | -200 to +300 | 1150-1700 | 195 | 190 | 180 | 171 | - | - | - | ≤ 0.09 | ≤ 0.7 | ≤ 1.0 | ≤ 0.04 | 0.015 | 16.0 18.0 | 6.5 7.8 | Al:0.7-1.5 | |||||
X5CrNiCuNb 16-4 SUS630 | -200 to +300 | 1150-1700 | 195 | 190 | 180 | 171 | - | - | - | ≤ 0.07 | ≤ 1.0 | ≤ 1.0 | ≤ 0.035 | 0.03 | 15.0 17.0 | 3.0 5.0 | ||||||
X8CrNiMoAl 15-7-2 | -200 to +300 | 1150-1700 | 195 | 190 | 180 | 171 | - | - | - | ≤ 0.09 | ≤ 1.0 | ≤ 1.0 | ≤ 0.04 | 0.03 | 14.0 16.0 | 6.5 7.75 | Mo: 2.0-3.0 Al:0.75-1.5 | |||||
Steel X39CrMo 17-1 |
-50 to +400 | 1200-1400 | 215 | 212 | 205 | 200 | 190 | - | - | 0.33-0.45 | ≤ 1.0 | ≤ 1.5 | ≤ 0.04 | 0.03 | 15.5 17.5 | ≤ 1.0 | Mo:0.7-1.3 | |||||
X 22CrMoV 12-1 | -50 to +500 | 1200-1400 | 216 | 209 | 200 | 190 | 179 | 167 | - | 0.18-0.24 | ≤ 0.5 | 0.4 0.9 | ≤ 0.025 | 0.015 | 11 12.5 | 0.3-0.8 | V:0.25-0.35 Mo:0.8-1.2 | |||||
X30WCrV53 SKD4 | -50 to +500 | ≥ 1470 | 216 | 209 | 200 | 190 | 179 | 167 | - | 0.25-0.35 | 0.15-0.30 | 0.20 0.40 | ≤ 0.035 | 0.035 | 2.2 2.5 | ≤ 0.35 | V:0.5-0.7 W: 4-5 | |||||
X40CrMoV5-1 SKD61 | -150 to +600 | 1650-1990 | 206 | 200 | 196 | 189 | 186 | 158 | - | 0.32 0.40 | 0.8 1.20 | 0.20 0.50 | ≤ 0.030 | 0.030 | 4.75 5.50 | V:0.80-1.20 Mo:1.1-.75 | ||||||
Nickel Inconel X750 |
-200 to +600 | ≥ 1170 | 214 | 207 | 198 | 190 | 179 | 170 | 158 | ≤ 0.08 | ≤ 0.50 | ≤ 1.0 | ≤ 0.02 | 0.015 | 14.0 17.0 | ≥ 70 |
Co≤ 1.0 Ti 2.25-2.75 Fe 5.0-9.0 | |||||
Inconel X718 | -200 to +600 | ≥ 1240 | 199 | 195 | 190 | 185 | 179 | 174 | 167 | 0.02 0.08 | ≤ 0.35 | ≤ 0.35 | ≤ 0.015 | 0.015 | 17.0 21.0 | 50.0 55.0 | V≤ 1.0 Mo:0.70-1.15 | |||||
Nimonic 90 | -200 to +700 | ≥ 1100 | 220 | 216 | 208 | 202 | 193 | 187 | 178 | ≤ 0.13 | ≤ 1.0 | ≤ 1.0 | ≤ 0.03 | 0.015 | 18.0 21.0 | Bal | V15.0-21.0 Mo:2.0-3.0 Al≤ 0.2 |
♦ 304 stainless steel
304 stainless steel is deformed by cold working to improve its elastic properties. It cannot be hardened by heat treatment. It will produce magnetism during cold working. 304 stainless steel has strong corrosion resistance and good physical properties.
♦ 316 stainless steel
316 stainless steel is deformed by cold working to improve its elastic properties, and cannot be hardened by heat treatment. It will produce magnetism during cold working. 316 stainless steel contains molybdenum, which has stronger corrosion resistance than 304 stainless steel, and can resist corrosion in chemical applications.
♦ 17-7PH (GH631, 0Cr17Ni7Al)
17-7PH similar corrosion resistance to 304 stainless steel, which can be precipitated by heat treatment and precipitation hardening. It has high tensile and yield strength. The fatigue performance is better than 304 stainless steel and 65Mn carbon steel. It also has good elasticity under ℃ environment.
♦ 15-7Mo (GH632, 0Cr15Ni7Mo2Al)
15-7MoHas similar corrosion resistance to 316 stainless steel. It can be precipitated by heat treatment and precipitation hardening. It has high tensile and yield strength, and its fatigue performance is better than 316 stainless steel and 65Mn carbon steel. It also has good elasticity under ℃ environment.
♦ Inconel X-750 (GH4145)
Inconel X-750 is a nickel-based precipitation hardening deformation superalloy. It mainly uses r'phase as the aging precipitation hardening phase. The recommended temperature is below 540℃. The alloy has certain corrosion resistance and oxidation resistance, and has certain low temperature performance.
♦ Inconel 718 (GH4169)
Inconel 718 is a nickel-based precipitation hardening deformation superalloy. The recommended temperature range is -253--600℃. The alloy has high strength below 600°C, has good fatigue resistance, radiation resistance, oxidation resistance and corrosion resistance, as well as good processing performance and long-term structural stability.
♦ A-286 (GH2132, SUH660)
Alloy A-286 is an iron-based precipitation hardening deformation high-temperature alloy. The recommended operating temperature is below 540℃. The alloy has high high and low temperature strength and long-term stability, good corrosion resistance and thermal deformation performance, and has good processing plasticity and satisfactory welding performance.